Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
Pyrotek Pyroboard™ S1000 Roller Pyroboard™ S1000 is designed to be used throughout the preheat and cooling sections of the furnace.Information provided by Pyrotek. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1119 P (SIS) Linear Block Copolymer Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 349 psi | |
Valley Adhesives EM-105 High Performance Application Glue Stick Valley Adhesives EM-105 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
Dow Corning 832 MULTI-SURFACE ADHESIVE SEALANT Neutral cure RTV sealant with very good adhesion to many substratesInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
Dow Corning HS III BASE & 10:1 CLEAR CATALYST High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Clear Catalyst is recommended f.. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
Dow Corning HS IV BASE & 10:1 COLORED CATALYST High strength lowest durometer silicone mold making rubber, suited for the production of print pads and for the detailed reproduction of fiines and art objects. HS IV Base with HS IV 10:1 Colored Ca.. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | |
BCC Products MB 1100 Polyurethane Foam Modeling Board MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or .. |
|||
Tensile Strength, Ultimate | 2.41 MPa | 350 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |