Polymer Property : Tensile Strength, Ultimate = 2.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.93 MPa
425 psi
Momentive Performance Materials TSE322 Light Blue Adhesive Sealant, Non-Corrosive Flowable
One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia..
Tensile Strength, Ultimate 2.93 MPa
425 psi
Momentive Performance Materials TSE322B Black Adhesive Sealant, Non-Corrosive Flowable
One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia..
Tensile Strength, Ultimate 2.93 MPa
425 psi
Zircar Refractory Composites RS-Cloth Refractory Sheet
Refractory Sheet RS-Cloth is ceramic fiber reinforced alumina composite. It offers the strength, durability, flexibility and versatility required by many high temperature applications up to 1300°C(..
Tensile Strength, Ultimate 2.93 MPa
425 psi
Zircar Refractory Composites RS-Tape Refractory Sheet
Refractory Sheet RS-Tape is ceramic fiber reinforced alumina composite. It offers the strength, durability, flexibility and versatility required by many high temperature applications up to 1300°C(2..