Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2000 MPa
290000 psi
Fiber only. Composites containing this fiber may have tensile strength of 1000 MPa.
Type P-VSB-32 (Union Carbide) Carbon Fiber
Pitch fibers are prepared by heating aromatic compounds above 350°C. A dehydrogenation condensation reaction occurs to form planar aromatic molecules which aggregate into a liquid crystalline phas..
Tensile Strength, Ultimate 2000 MPa
290000 psi
Fiber only. Composites containing this fiber may have tensile strength of 1000 MPa.
Type P-VS-0053 (Union Carbide) Carbon Fiber
Pitch fibers are prepared by heating aromatic compounds above 350°C. A dehydrogenation condensation reaction occurs to form planar aromatic molecules which aggregate into a liquid crystalline phas..
Tensile Strength, Ultimate 2000 MPa
290000 psi
China Tungsten YG9X Tungsten Carbide Powder
Information provided by China Tungsten
Tensile Strength, Ultimate 2000 MPa

@Thickness 25.4 mm
290000 psi

@Thickness 1.00 in
filament
3M Nextel™ 440 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural ap..
Tensile Strength, Ultimate 2000 MPa

@Thickness 25.4 mm
290000 psi

@Thickness 1.00 in
gauge filament
3M Nextel™ 550 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural applications w..