Polymer Property : Tensile Strength, Ultimate = 2000.00 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3421 - 13.7895 MPa

@Temperature 100 - 121 °C
1500.00 - 2000.00 psi

@Temperature 212 - 250 °F
Average value: 12.0 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 10.3421 - 13.7895 MPa

@Time 605000 - 605000 sec
1500.00 - 2000.00 psi

@Time 168 - 168 hour
Average value: 12.0 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..