Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1392 MPa
201900 psi
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..