Polymer Property : Tensile Strength, Ultimate = 20600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Kolon KOPET® KP133G45 FR-PET Resin
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of..
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 142 MPa
20600 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Tensile Strength, Ultimate 142 MPa

@Temperature 871 °C
20600 psi

@Temperature 1600 °F
ASTM E8
ATI Allegheny Ludlum 309S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..