Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2070 MPa
300000 psi
55 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
EDRO #8 Premium 420 Stainless Mold Steel
EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in..
Tensile Strength, Ultimate 2070 MPa
300000 psi
hardened to 52 HRC
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel
Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng..