Polymer Property : Tensile Strength, Ultimate = 20700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 143 MPa
20700 psi
ISO 527-1, 2
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 143 MPa
20700 psi
ISO 527-1, 2
Polyplastics Duranex® 353RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 143 MPa
20700 psi
5 mm/min
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..
Tensile Strength, Ultimate 143 MPa
20700 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 143 MPa

@Temperature 538 °C
20700 psi

@Temperature 1000 °F
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc..
Tensile Strength, Ultimate 143 MPa
20700 psi
5mm/min; ISO 527
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT
Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement.