Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 - 143 MPa
18200 - 20700 psi
Average value: 133 MPa Grade Count:3
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..