Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.6 MPa | 2120 psi | GB/T 528 |
Chengdu Polyster 9502 High Performance Grade TPV Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd. |