Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1471 MPa | 213400 psi | 0° Fiber Direction; ASTM D3039 |
Saint-Gobain Quartzel® Fiber/Cyanate Ester Resin Unidirectional Composite Fiber: Quartzel® Silica Roving C9 667 QS16 (33). Resin: YLA RS-3C.Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous,.. |