Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1200 - 1490 MPa | 174000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 1200 - 1490 MPa | 174000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/2HT (TH02) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 73%Superficial Hardness: 30N 58-6.. |
|||
Tensile Strength, Ultimate | 1200 - 1490 MPa | 174000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1200 - 1490 MPa | 174000 - 216000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Tensile Strength, Ultimate | 1270 - 1490 MPa | 184000 - 216000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |