Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1515 MPa
219700 psi
Haynes 214® alloy, 50% cold reduction
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1515 MPa

@Temperature 427 °C
219700 psi

@Temperature 800 °F
3 in bar
Carpenter Pyrotough® 78 Hot Work Die Steel
Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented c..