Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1540 MPa
223000 psi
Haynes 625 alloy, 50% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..