Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 - 225 MPa

@Temperature 60.0 - 230 °C
8700 - 32600 psi

@Temperature 140 - 446 °F
Average value: 107 MPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..