Polymer Property : Tensile Strength, Ultimate = 231 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 231 MPa
>= 33500 psi
Typical for SiC
Destech Silicon Carbide, Solid or Foamed
Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c..