Polymer Property : Tensile Strength, Ultimate = 234000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1610 MPa
234000 psi
SSAB Tunnplat Domex® 044 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..