Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Sylvin Technologies 8600-75 Clear PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Sylvin Technologies 8950-85 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Sylvin Technologies 9600-75 Clear PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Sylvin Technologies 9950-85 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Die C (35 min / 145°C); ASTM D412
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
SE BR-1220M is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production..
Tensile Strength, Ultimate 16.2 MPa
2350 psi
ASTM D638
Colorite Polymers 8033 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 16.2 MPa
2350 psi
ASTM D638
Colorite Polymers 8033SF General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 16.2 MPa
2350 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8505 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **)
FormulationViton® 8505