Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1630 MPa
237000 psi
hardness of 48 HRC
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic..