Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2400 MPa
348000 psi
Cytec Thornel® P-100 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.0.32 m/g yield, 0 or 32 tpm t..
Tensile Strength, Ultimate 2400 MPa
348000 psi
Cytec Thornel® P-120 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.2000 filaments/strand, 0.33 m..
Tensile Strength, Ultimate 2400 MPa
348000 psi
China Tungsten YG11 Tungsten Carbide Powder
Information provided by China Tungsten
Tensile Strength, Ultimate 2400 MPa
348000 psi
China Tungsten YG13X Tungsten Carbide Powder
Information provided by China Tungsten
Tensile Strength, Ultimate 2400 MPa
348000 psi
China Tungsten YG25C Tungsten Carbide
Information provided by China Tungsten
Tensile Strength, Ultimate 2400 MPa
348000 psi
China Tungsten YG9C Tungsten Carbide Powder
Information provided by China Tungsten