Polymer Property : Tensile Strength, Ultimate = 25500.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 - 175.816 MPa

@Temperature -40.0 - 93.3 °C
8700 - 25500.0 psi

@Temperature -40.0 - 200 °F
Average value: 80.8 MPa Grade Count:16
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..