Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 178 MPa | 25800 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |