Polymer Property : Tensile Strength, Ultimate = 26.63 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.05 - 26.63 MPa

@Temperature 70.0 - 100 °C
587 - 3862 psi

@Temperature 158 - 212 °F
Average value: 53.1 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..