Tensile Strength, Ultimate 18.58 MPa
2695 psi
ASTM D638
Colorite Polymers 8577 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..