Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.3 MPa | 3950 psi | |
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |