Tensile Strength, Ultimate 77.0 - 281.306 MPa

@Temperature -40.0 - 150 °C
11200 - 40800.1 psi

@Temperature -40.0 - 302 °F
Average value: 104 MPa Grade Count:4
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..