Polymer Property : Tensile Strength, Ultimate = 2820 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.4 MPa
2820 psi
Cured
KKPC KOSYN KBR 01 Polybutadiene Rubber (High cis BR)
Polybutadiene Rubber (High cis BR)Characteristics: Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solut..