Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 19.7 MPa | 2850 psi | |
Sylvin Technologies 8600-90 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 19.7 MPa | 2850 psi | |
Sylvin Technologies 6140-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 19.7 MPa | 2850 psi | ASTM D412 |
Colorite Polymers CS1535UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |