Tensile Strength, Ultimate 289 MPa
41900 psi
ASTM D638
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert..