Tensile Strength, Ultimate 3.10 MPa
450 psi
ISO 37
Multibase TPSiV® 4000-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Tensile Strength, Ultimate 3.10 MPa
450 psi
TPE-0153 (ASTM D 412)
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe..
Tensile Strength, Ultimate 3.10 MPa
450 psi
ASTM D638
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications.
Tensile Strength, Ultimate 3.10 MPa
450 psi
Dow Corning HS II BASE & 10:1 CLAY CATALYST
High strength silicone mold making rubber, suited for the art foundry industry that typically uses sulfur-based clays. HS II Base with HS II 10:1 Clay Catalyst is recommended for use with polyesters..
Tensile Strength, Ultimate 3.10 MPa
450 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Strength, Ultimate 3.10 MPa
450 psi
Cured property; ASTM D412
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect..
Tensile Strength, Ultimate 3.10 MPa
450 psi
TM R050-36
Resinlab® SEC1233 Silver Filled Epoxy Adhesive