Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 214 MPa | 31000 psi | |
Pacific Sintered Materials CU-143-W Copper Powdered Metal Applications: High electrical and thermal conductivity. Good for heat sinks and electrical components.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 214 MPa | 31000 psi | |
PSM Industries Pacific Sintered Metals Copper CU-143-W Powdered Metal High electrical and thermal conductivity, Good for heat sinks and electrical problemsInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 214 MPa @Temperature 982 °C |
31000 psi @Temperature 1800 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 214 MPa | 31000 psi | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 214 MPa | 31000 psi | Annealed |
CMW® D57F Silver Iron Contact Material For electrical contacts; AC resistive loads.Information provided by CMW Inc. |