Polymer Property : Tensile Strength, Ultimate = 3130 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.6 MPa
3130 psi
500mm/min; ASTM D638
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D638
KKPC Kuhmo HI 425EP Extrusion Molding HIPS
Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerization of styrene mono..
Tensile Strength, Ultimate >= 21.6 MPa

@Temperature 100 °C
>= 3130 psi

@Temperature 212 °F
Sibur SKI-3 Superior Quality, 1st Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment.
Tensile Strength, Ultimate >= 21.6 MPa

@Temperature 100 °C
>= 3130 psi

@Temperature 212 °F
Sibur SKI-3 Superior Quality, 2nd Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment.
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D638
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic
SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo..
Tensile Strength, Ultimate >= 21.6 MPa

@Temperature 100 °C
>= 3130 psi

@Temperature 212 °F
Sibur SKI-3S Superior Quality, 1st Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. It is used instead of natural rubber during production of colored rubber articles, medical articles, and rubbers contacting with food products.
Tensile Strength, Ultimate >= 21.6 MPa

@Temperature 100 °C
>= 3130 psi

@Temperature 212 °F
Sibur SKI-3S Superior Quality, 2nd Group Isoprene Rubber (IR)
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. It is used instead of natural rubber during production of colored rubber articles, medical articles, and rubbers contacting with food products.
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D638
SK Chemicals SKYPEL G130D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D412
Lubrizol Estane® T465A Thermoplastic Polyurethane
Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
Tensile Strength, Ultimate 21.6 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
3130 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate
Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D412
Lubrizol Estane® CR185A Thermoplastic Polyurethane
Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..