Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 216 MPa | 31300 psi | |
Shinil Chemical SHINCON PA66 Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Tensile Strength, Ultimate | 216 MPa | 31300 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Tensile Strength, Ultimate | 216 MPa | 31300 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G8-43GF Nylon 66, 43% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |