Polymer Property : Tensile Strength, Ultimate = 320 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 320 MPa

@Temperature 600 °C
46400 psi

@Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 320 MPa

@Temperature 600 °C
46400 psi

@Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 320 MPa

@Temperature 600 °C
46400 psi

@Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
Tensile Strength, Ultimate 320 MPa

@Temperature 870 °C
46400 psi

@Temperature 1600 °F
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
SSAB Tunnplat Domex® 220YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Ultimate 320 MPa
46400 psi
Wieland 1945 Wilaform Platinum
Platinum alloy for universal use.Applications: chains, coin/shape, laminar decoration, pipes, tubingDental
Tensile Strength, Ultimate 320 MPa
46400 psi
Wieland 3011 Wilaform Silver
Universally applicable silver alloyApplications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Tensile Strength, Ultimate 320 - 400 MPa
46400 - 58000 psi
CLAL-MSX CUPROROR® TL1 1/4 hard, Copper Alloy
Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat..
Tensile Strength, Ultimate 320 - 400 MPa
46400 - 58000 psi
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Tensile Strength, Ultimate 320 MPa

@Temperature 371 °C
46400 psi

@Temperature 700 °F
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 210), SAE J2340 Type 210 B
Information provided by AK Steel
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 250)
Information provided by AK Steel
Tensile Strength, Ultimate >= 320 MPa
>= 46400 psi
Minimum
Aleris Weldural Aluminum Alloy, 400 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Tensile Strength, Ultimate 320 - 370 MPa
46400 - 53700 psi
ArcelorMittal 14 High formability steel for drawing, Hot rolled
Available in the following: uncoated (DD14) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au..
Tensile Strength, Ultimate 320 MPa

@Temperature 150 °C
46400 psi

@Temperature 302 °F
Typical, after 10,000 hours
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..