Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.11 MPa
3352 psi
s.d. 2.17 MPa, test specimen 1.23 cm wide (s.d. 0.008 cm), 0.21 cm thick (s.d. 0.008 cm)
Schmelzer Industries Curveil 220-30 Fiberglass Veil
Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. ..