Polymer Property : Tensile Strength, Ultimate = 350 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 350 MPa
39200 - 50800 psi
SSAB Tunnplat Docol® DC04 (Fe P04) Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 270 - 350 MPa
39200 - 50800 psi
SSAB Tunnplat Docol® DC06 (Fe P06) Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 270 - 350 MPa
39200 - 50800 psi
ArcelorMittal 15 High formability steel for drawing, Hot rolled
Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru..
Tensile Strength, Ultimate 270 - 350 MPa
39200 - 50800 psi
ArcelorMittal 16 High formability steel for drawing, Hot rolled
Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru..
Tensile Strength, Ultimate 260 - 350 MPa
37700 - 50800 psi
ArcelorMittal 54+AS Aluminized steel
Use: Difficult drawingInformation provided by ArcelorMittal
Tensile Strength, Ultimate 260 - 350 MPa
37700 - 50800 psi
ArcelorMittal 56+AS Aluminized steel
Use: Extra-deep drawingInformation provided by ArcelorMittal
Tensile Strength, Ultimate 260 - 350 MPa
37700 - 50800 psi
ArcelorMittal 57+AS Aluminized steel
Use: Extra-deep drawingInformation provided by ArcelorMittal