Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.250 - 2.50 MPa | 36.3 - 363 psi | |
MetaFoam Copper-Silver Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Tensile Strength, Ultimate | 0.250 MPa | 36.3 psi | ASTM D3574E |
Covestro Bayfill® 370 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Closed Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |