Polymer Property : Tensile Strength, Ultimate = 361 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.20 - 361 MPa
319 - 52400 psi
Average value: 143 MPa Grade Count:46
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..