Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 13.7 - 37.3 MPa | 1990 - 5400 psi | ASTM D638 |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Tensile Strength, Ultimate | 9.80 - 37.3 MPa | 1420 - 5410 psi | Average value: 23.1 MPa Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |