Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.8 MPa
3740 psi
508 mm/min; ASTM D638
Dow Engage® 8480 Polyolefin Elastomer
Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari..