Polymer Property : Tensile Strength, Ultimate = 3790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 26.1 MPa
>= 3790 psi
ISO 1184-1983E
LyondellBasell Montell 0300 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive..
Tensile Strength, Ultimate 26.1 MPa
3790 psi
Vulcanizate, Press cured, TC95 +3min at 180°C
Dow Nordel® IP 4770P Heat Resistant Peroxide Compound
FormulationNordel® IP 4770P
Tensile Strength, Ultimate 26.1 MPa
3790 psi
Vulcanizate, Press cured, TC95 +3min at 180°C
Dow Nordel® IP 4770R Heat Resistant Peroxide Compound
FormulationNordel® IP 4770R