Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 40.2 MPa | 5830 psi | ASTM D412 |
SK Chemicals SKYTHANE® 595A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 40.2 MPa | 5830 psi | ASTM D412 |