Polymer Property : Tensile Strength, Ultimate = 403 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 403 MPa

@Temperature 760 °C
58500 psi

@Temperature 1400 °F
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Tensile Strength, Ultimate 403 MPa
58500 psi
Annealed
Special Metals Nickel 201
Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)...
Tensile Strength, Ultimate 403 MPa
58500 psi
Typical Annealed
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201
Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c..