Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 419 MPa
60800 psi
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..