Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.5 MPa
6160 psi
ASTM D638
Tipco Tipcolite® TG 311 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie..