Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.0 - 43.0 MPa
1450 - 6240 psi
Average value: 21.4 MPa Grade Count:141
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 31.0 - 43.0 MPa

@Temperature 180 - 180 °C
4500 - 6240 psi

@Temperature 356 - 356 °F
Average value: 68.8 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 31.0 - 43.0 MPa

@# of Cycles 100000 - 1.00e+7
4500 - 6240 psi

@# of Cycles 100000 - 1.00e+7
Average value: 68.8 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 31.0 - 43.0 MPa

@Temperature 180 - 180 °C
4500 - 6240 psi

@Temperature 356 - 356 °F
Average value: 70.2 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Tensile Strength, Ultimate 31.0 - 43.0 MPa

@# of Cycles 100000 - 1.00e+7
4500 - 6240 psi

@# of Cycles 100000 - 1.00e+7
Average value: 70.2 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..