Polymer Property : Tensile Strength, Ultimate = 430.001 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.96475 - 43.5749 MPa

@Temperature -40.0 - 85.0 °C
430.001 - 6320.01 psi

@Temperature -40.0 - 185 °F
Average value: 23.0 MPa Grade Count:1
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..