Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3090 MPa | 448000 psi | |
Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Tensile Strength, Ultimate | 3090 MPa | 448000 psi | |
Toho Tenax Besfight® MC Type II (3000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Tensile Strength, Ultimate | 3090 MPa | 448000 psi | |
Toho Tenax Besfight® MC Type II (6000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |