Polymer Property : Tensile Strength, Ultimate = 464 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 464 MPa
67300 psi
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel
The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi..