Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.24 MPa | 470 psi | |
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Tensile Strength, Ultimate | 3.24 MPa | 470 psi | |
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |